THREE BOND INTERNATIONAL, INC.
This company has introduced TB2202, TB2206 and TB2274B, designed for under-filling applications. These products feature good flow and penetration. They also offer a fast setting time at 150degC and can be stored in the refrigerator. Circle No. 110