An anaerobic sealant on the other hand is always supplied in a thin-walled plastic bottle or tube that is usually only half filled. This plastic is usually low-density polyethylene, which is highly permeable to oxygen. Anaerobics, as their name implies, only cure when oxygen is excluded, like inside an assembled joint, and are also accelerated by certain metals such as iron or copper, which usually come from the surfaces being assembled.