ANGUS Chemical Company has developed the ACCELACURE Fast Cure Novolac System, a breakthrough technology that delivers the processing performance of polyester combined with the flame, smoke and smoke toxicity (FST) performance of a phenolic. The first ACCELACURE system application - ACCELACURE PT 1.0 for pultrusion - is now commercially available. ACCELACURE Fast Cure Novolac System PT 1.0 for pultrusion provides a number of benefits over competitive materials, including improved mechanical performance, fast and easy processing rates, and unmatched FST performance. ACCELACURE PT 1.0 may be used instead of existing fire-resistant resins, such as phenolic resoles, modified acrylic, urethanes (MODAR) and fire-resistant polyesters.