Hydrogenated Styrenic Block Copolymer Offers Benefits for PSAs
A new, hydrogenated styrene block copolymer provides a good balance of properties for various adhesive applications.
The focus of this article is on the potential of a novel hydrogenated KRATON polymer, called KRATON GRP-6924, for pressure sensitive adhesives (PSAs) in tapes and labels. Application of this new polymer in adhesive formulations for nonwovens has been presented previously3.