This article focuses on the use of paste dot for the binding of nonwovens to themselves and other substrates.
Interfiber adhesion is created by mechanical, chemical, thermal or solvent means, or by various combinations of these processes. Table 1 shows some of the methods that can be used for combining nonwovens.