Scapa Medical now offers Bioflex Rx869S, a double-coated fabric pressure-sensitive adhesive tape specifically designed for direct skin applications, such as bandages, EKG electrodes and TENS. Rx869S consists of a 25 mil white spunlaced polyester fabric, double-coated on each side with a unique pressure-sensitive acrylic adhesive. The tape is supplied on an easy release 80# white kraft paper liner that provides stay-flat properties for easy die-cutting. Lightweight and comfortable, this fabric tape provides excellent conformability to curved areas of the body. The product delivers good adhesion to skin, yet removes cleanly without causing trauma.