Elkhart, IN-based Startracks specializes in building custom mobile vehicles used as medical clinics, law-enforcement command posts and motorcycle transport units. The company also manufactures mobile homes for wheelchair-bound customers. These handicapped-accessible vehicles contain such features as extra-wide doors and center aisles and bathrooms large enough to accommodate wheelchairs. ARALDITE 2011 epoxy adhesive supports Startracks in the production of different vehicle designs because it bonds wood, metal and FRP substrates quickly and effectively. Once cured, the adhesive features a lap-shear strength of 2,560 psi and roller peel strength of 28 pli; it also exhibits good resistance to static and dynamic loading.