Penford Products has teamed up with Elmer’s to develop natural school glues.
Penford Products, a division of Penford Corp. and a leading global supplier of specialty bio-products for use in industrial applications including coatings, adhesives and polymers, has announced its support behind the launch of a natural school glue jointly developed with Elmer’s Products Inc. The natural glue, marketed as Elmer’s School Glue Naturals™, uses Penford’s proprietary PenFlex™ technology.
Elmer’s pourable School Glue Naturals reportedly comprises 99% natural ingredients and is made from renewable plant-based resources. The adhesive is safe, non-toxic and washable, and was designed to apply and dry clear to meet parents’ and teachers’ needs for school products.