This company’s UK distributor, Techsil, has introduced a new adhesives with improved conductivity to the UK market. Panacol has expanded its Elecolit® product portfolio to include adhesives with improved conductivity. The adhesives can reportedly be applied by jetting.
The new silver-filled adhesives are both electrically and thermally conductive, and available in a range of viscosities. The one- and two-part conductive adhesives are suitable for shielding and ESD protection; electrically conductive contacting and bonding of conducting paths within the electronic field; and electrically conductive bonding on circuit boards and PCBs.