This company now offers Lord Corp.’s acrylic adhesive system, Lord 810/20. The adhesive system was reportedly designed to remove the problem of ‘read-through’ where the surface of a bonded substrate has become visibly distorted because of stresses that occurred during the curing process.
The adhesive reportedly works in conjunction with Lord Accelerator 20 and, upon curing, can create a flexible system for bonding metals and engineered plastics. This adhesive system reportedly provides a high speed cure, and strong bonding with virtually no bond-line read through. In addition, the use of Lord Accelerator 20 can enable precise control of the adhesive bond-line thickness, thanks to the glass beads in the material.