Advanced Polymer Monitoring Technologies Inc. recently announced that its automatic continuous online monitoring of polymer reactions (ACOMP) product for industrial scale polymer production monitoring has been installed and operating in a polymer facility since 2014.
ACOMP technology was developed through R&D and lab use over 17 years, with more than 50 peer-reviewed publications and a number of patents from Tulane University’s Center for Polymer Reaction Monitoring and Characterization (PolyRMC). This reportedly marks the first time the technology has been used for Industrial reactor monitoring and control.