A new adhesive is available from the Vitralit® UV 4050s series: Vitralit UV 4050 MV. The UV adhesive reportedly features medium viscosity with 450 to 650 mPas and is suited for bonding plastics, especially for med-tech applications and medical device assembly. When cured, it shows flexibility and stability. This transparent adhesive reportedly has shrinkage of only 2%.
The adhesive can provide adhesion to most plastics like PVC, ABS, SAN and PC, as well as to stainless steel and glass. If at least one assembly material is transparent, it will cure quickly to produce a strong and reliable bond. UV blocked materials like polycarbonate can be cured because the adhesive has the ability to cure with visible light (>400nm).