This company has launched a new series of high-tack acrylic double-coated tapes and transfer adhesives. Developed with the company’s solvent-free, 100%-solids adhesive technology, the product series features Mactac’s new high-tack acrylic adhesive, MP410. The adhesive is reportedly easy to handle and die-cut and was designed to perform well on a variety of substrates, including acrylonitrile butadiene styrene (ABS), metals, polycarbonate, most foams, fabrics and high density polyethylene (HDPE).
The MP410 adhesive reportedly has low levels of VOCs, migratory compounds, and residuals. It can deliver strong optical properties, adhesion performance superior to many traditional solvent acrylics, solvent, chemical and plasticizer resistance, UV-resistance, and wide performance range.