Emery Oleochemicals recently announced it has opened a new pilot plant in Loxstedt, Germany.
Emery Oleochemicals recently announced it has opened a new pilot plant in Loxstedt, Germany. The facility reportedly is intended to give the GPA team greater flexibility in upscaling products.
The pilot plant reportedly complements TDC to provide combined technical capabilities in manufacturing environmentally friendly polymer additives used in markets such as automotive, construction, electronics, packaging, and toys and sports equipment.