This company has introduced a new adhesive for optoelectronic applications. DELO DUALBOND OB786 can be used for fixing components within seconds, while ensuring precision and high strength.
This milky epoxy resin, with medium viscosity, can be used for fixing and bonding optoelectronic components. It reportedly ensures good adhesion to common substrates like aluminum, FR4, PPS and LCP.