Ashland Completes Facility Acquisition from Reichhold
The facility employs approximately 50 people.
Ashland Global Holdings Inc. recently completed the acquisition of the manufacturing facility in Etain, France, from Reichhold. The facility, which employs approximately 50 people, manufactures unsaturated polyester resins (UPR) used in a variety of end markets.
Reportedly an investment of over $1 million was invested in the new lab facilities and equipment, which includes devices for resins characterization, viscosity and thickening measurement, surface analysis, and mechanical properties, as well as a 1,000 KN press.
“With the new lab, Ashland can accelerate new product development, innovation and validation of products before launch. The lab will be able to replicate exact customer conditions will significantly reduce the time-to-market for our products,” said Allessandro Lago, director of sales, EMEA.