PHOTOBOND GB4033 can be used in wearables and consumer electronics. The new light-curing acrylate is reportedly designed for material joints that require adhesives to be strong, flexible and tight. The low-viscous, one-component, solvent-free acrylate can provide sealing properties against water, humidity and dust. It can be used in temperatures ranging from -40°C to 120°C.
Featuring an elongation at tear of 400%, the adhesive is suggested to be an extremely flexible, tension-equalizing product. Its elasticity also reportedly allows for good peel resistance on glass and plastic.