Answer: These materials do not cause any problems when used in thermoset plastics. However, some thermoplastics plastics are stress-cracked by the monomers used in these adhesives through a phenomenon often called liquid-induced crystallization. This phenomenon is made worse as the liquid threadlocker is in contact with the plastic for a longer time before it cures to a solid, and if the plastic is stressed.