This company recently announce plans to introduce Aroset™ Gentle 700, a new medical pressure-sensitive adhesive (PSA) at MD&M West, taking place February 5-7 in in Anaheim, Calif. The PSA was reportedly developed for medical use, to be skin friendly with good breathability and to allow for minimal pain and trauma upon removal.
“We are excited to introduce this product for the wound-care market, as well as the medical device industry,” said Todd McMillen, global industry manager, PSA. “Aroset Gentle 700 PSA provides a better end-user experience as it allows for minimal trauma upon removal, especially for more sensitive skin individuals.”