ACEMATT® 3400 is a new matting agent in the ACEMATT line, specially developed for high-transparency clear coatings and soft-touch coatings with smooth surfaces. The surface-treated, thermal silica has a medium-particle size of 7.5 µm. Improved grind performance reportedly results in a smooth surface finish with outstanding optical and haptic properties.
This silica is intended for use in clear coatings and water- and solvent-based coatings. Typical application fields include wood coatings, plastics and automotive coatings. In addition, it can be used in high-solids and low-VOC formulations.