The one-component, non-sag, elastomeric silicone can be used for general sealing and bonding applications.
Sikasil® GP-101 is a general-purpose, acetoxy cure silicone sealant that reportedly meets the requirements of ANSI/NSF Standard 51 for direct food contact. The one-component, non-sag, elastomeric silicone can be used for general sealing and bonding applications. It reportedly maintains elastomeric properties up to 300°F continuous, 350°F intermittent.
The sealant reportedly offers joint movement of -/+ 25% capability (tested to ISO 11600) and has adhesion to many substrates without priming. Typical substrates include aluminum, fiberglass, plastic, glass, tile, ceramic, wood, and painted metals.