Specially engineered for curing at temperatures lower than the current standard of 180-190°C, the new offering is TGIC-free polyester, which reportedly saves energy and helps customers to improve their efficiency.
AkzoNobel recently announced that it has launched smooth-finish additions to its range of Interpon powder coatings low-emissivity (low-e) products. The company introduced a coarse texture range of low-e products late last year. Specially engineered for curing at temperatures lower than the current standard of 180-190°C, the new offering is TGIC-free polyester, which reportedly saves energy and helps customers to improve their efficiency.
Designed for a wide range of customers, including industrial manufacturers of steel constructions, street and garden furniture, and agricultural and construction equipment, a total of 50 smooth products are included in the range; gloss, satin, and matt finishes are available. The new Interpon low-e range is initially being launched in Europe, with plans in place to launch in other regions in the future.