This website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
This Website Uses Cookies
By closing this message or continuing to use our site, you agree to our cookie policy. Learn More
This website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
Adhesives Mag logo
search
cart
facebook twitter linkedin youtube
Adhesives Mag logo
  • NEWS
    • Adhesives & Sealants Headlines
    • Mergers/Acquisitions
    • Events Calendar
    • Market Trends
    • Price Adjustments
  • PRODUCTS
  • TOPICS
    • Finished Adhesives and Sealants
    • Pressure-Sensitive Adhesives (PSAs)
    • Coatings
    • Raw Materials and Chemicals
    • Materials Handling/Processing
    • Meter/Mix/Dispense
    • Curing
    • Testing/Quality Control
    • Packaging of Adhesives & Sealants
    • Converting/Packaging
    • Composites
    • Sustainability
  • COLUMNS
    • Ask Dr. Dave
    • Strategic Solutions
    • IP in Depth
    • Tape Talk
  • TOP 20
  • MULTIMEDIA
    • Videos
    • Podcasts
    • Photo Galleries
    • Webinars
    • Mobile App
  • EXPLORE
    • Blog
    • ASI Store
    • Industry Links
    • Market Research
  • DIRECTORIES
    • Buyers' Guide
    • Global Adhesives & Sealants Directory
    • Raw Materials, Chemicals, Polymers and Additives Handbook
    • Equipment Handbook
    • Distributor Directory
    • Take A Tour
  • MAGAZINE
    • Current Issue
    • Digital Edition
    • Advertiser Index
    • Classifieds & Services Marketplace
  • ADVERTISE
    • Contact
    • Custom Content & Marketing Services
  • SUBSCRIBE
    • eNewsletter
    • Online Registration
    • Customer Service
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Home » BYK-GARDNER: Color, Gloss, and Surface Texture Analyzer

You have 0 Articles Left This Month. Register Today for Unlimited Access.

Adhesives and Sealants TopicsTesting/Quality Control

BYK-GARDNER: Color, Gloss, and Surface Texture Analyzer

Like our visual judgement, the new spectro2profiler reportedly measures color, gloss, and surface structure simultaneously in a robust, portable tool.

September 15, 2020
Order Reprints
No Comments

BYK-Gardner recently announced the launch of its new spectro2profiler, an instrument to measure color and gloss, as well as the 3D topography of the surface texture. Visual quality perception is influenced by color, gloss, and the surface structure. Like our visual judgement, the new spectro2profiler reportedly measures all three parameters simultaneously in a robust, portable tool.

The spectro2profiler uses a circumferential illumination at 45° with 0° viewing. The company reports that an extra-large measurement spot with homogenous illumination guarantees highly repeatable and representative readings. High accuracy and inter-instrument agreement are reportedly ensured, enabling the use of digital standards.

You have 0 complimentary articles left.

Register for free today to continue reading!

Already have an account? Sign in here.

Privacy Policy

Related Articles

BYK-GARDNER: Updated Data Analysis Software

Cassell and Kowalski Assume New Roles at BYK-Gardner

ALTANA Acquires Paul N. Gardner

ALTANA Enters Software as a Service Domain with Acquisition of Office Color Science

Related Directories

BYK-Gardner USA

BYK-Gardner USA

BYK-Gardner USA

Subscribe For Free!
  • Digital Edition Subscription
  • eNewsletter
  • Online Registration
  • Subscription Customer Service

More Videos

Popular Stories

Henkel Nicolas Krauss

Henkel Personnel Announcement Draws Massive Reader Interest

COVID-19

Are Antimicrobial Coatings Effective in the Fight Against COVID-19?

Headlines.jpg

DuPont Board Approves Separation of Nutrition & Biosciences Business through Exchange Offer

Picture-4

Printed Electronics: Enabling Remote Healthcare and Enhancing Patient Treatment

ASI Top 20 website

Events

February 8, 2021

Kitchen & Bath Industry Show

Virtual in 2021, the Kitchen & Bath Industry Show (KBIS) is North America’s largest trade show dedicated to all aspects of kitchen and bath design.
February 8, 2021

International Builders’ Show

Virtual in 2021 and marking its 77th year, the National Association of Home Builders (NAHB) International Builders’ Show® connects, educates, and improves the residential construction industry.

View All Submit An Event

Products

Handbook of Sealant Technology

Handbook of Sealant Technology

The Handbook of Sealant Technology provides an in-depth examination of sealants, reviewing their historical developments and fundamentals, adhesion theories and properties, and today’s wide range of applications.

See More Products

COVER-144px

2019 Buyers' Guide

Your comprehensive buyers’ guide for raw materials, distributors, equipment, services, and finished adhesives and sealants.

The latest news and information

Content focused on adhesive & sealant manufacturing, formulations and finished products

SUBSCRIBE TODAY
  • Resources
    • List Rental
    • Ad Index
    • Classifieds & Services Marketplace
    • Want More?
    • Connect
    • Online Extras
    • Manufacturing Group
    • Privacy Policy
    • Survey And Sample
  • Subscribe
    • Digital Subscription
    • eNewsletters
    • Customer Service
  • Privacy
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2021. All Rights Reserved BNP Media.

Design, CMS, Hosting & Web Development :: ePublishing