AkzoNobel to Build New Powder Coatings Plant in Taiwan
The fully automated plant represents a €20 million (approximately $23.6 million) investment.
AkzoNobel recently held a groundbreaking for a new state-of-the-art and sustainable powder coatings plant in Chungli, Taiwan. The fully automated plant, which represents a €20 million (approximately $23.6 million) investment, will have the increased production capacity to fulfill growing demand in the architecture, auto accessories, telecommunications, electronic components, furniture, domestic appliances, sports equipment, and machine tools markets.
Once operational, AkzoNobel expects that the new plant will bring the company closer to its overall energy and water sustainability ambitions. The plant is expected to reduce energy consumption by 30%, increase the water reuse rate to 60%, and achieve zero volatile organic compound (VOC) emissions, in addition to creating a safer and healthier working environment.
“The COVID-19 pandemic has brought a lot of uncertainties to global markets,” said Fred Moreux, director of Manufacturing for Asia at AkzoNobel. “Investing in a new plant in Taiwan at this critical time will help us streamline our supply chain while setting a new benchmark in the local paints and coatings industry.”