Bonding Study Evaluates Performance of Avery Dennison Adhesives with Woodbridge Flexible Foams
This study focused on Woodbridge AutoBond flexible foams, which can be found in automotive applications such as acoustics, seating, and interior and overhead systems.
Avery Dennison Performance Tapes recently released the second in a series of bonding studies that reportedly make it easier for converters to evaluate the performance of Avery Dennison Core Series™ adhesive products with commonly used materials. This study focused on Woodbridge AutoBond™ flexible foams, which can be found in automotive applications such as acoustics, seating, and interior and overhead systems.
The study was performed in collaboration with Woodbridge at the Avery Dennison Performance Tapes Painesville Innovation Center, an ISO 17025-certified facility that reportedly tests under real-world and extreme conditions with tight control of environmental conditions. The study evaluated Core Series adhesives using two different laminating methods on Woodbridge AutoBond products. Samples were tested at 180° peel adhesion at 12 in./min.