PANACOL: UV Adhesive for Decorations and Dome Coatings
Vitralit UC 6685 is a transparent, UV-curing adhesive based on epoxy resin.
Vitralit® UC 6685 was reportedly formulated by Panacol specifically for decorations on plastic, glass, and metal. Due to its slight magnifying property, the transparent adhesive reportedly produces a high-quality image of the structures and illustrations underneath.
Vitralit UC 6685 is a transparent, UV-curing adhesive based on epoxy resin. Panacol reports that the viscosity of the one-component, easy-to-dispense adhesive makes it suitable for decorative applications on flacons and bottles or for dome coatings, an elegant protective coating for products such as key rings, lapel pins, buttons, name tags, pens, and jewelry.