Applications include electronic transformers, inductors, sensors, oceanic equipment, and aerospace components.
Creative Materials recently introduced 904-64A/B, a two-component silicone addition-cured potting compound. According to the company, this high-performance product is red in color and thermally conductive, cures at room-temperature, and has low shrinkage. In addition, it features easy air release as well as excellent mechanical, thermal, and shock resistance properties.
904-64A/B has a wide service temperature range and excellent chemical resistance. It has a rating of UV 94V-0 and when fully cured will not undergo reversion under normal operating conditions.