The high-temperature-resistant adhesive has been optimized for bonding magnets in electric motors.
DELO has launched DELO MONOPOX HT2999, a structural adhesive with high temperature stability. According to the company, the adhesive achieves compression shear strength of 20 MPa at 180°C.
Developed primarily for use in the automotive industry and mechanical engineering, these high-temperature-resistant adhesives are reportedly in demand for use with electric motors and power electronics. According to the company, many products that are currently on the market show a clear drop in performance at temperatures above 150°C. DELO’s new structural adhesive can be used above that temperature.