ENGINEERED POLYMER SOLUTIONS (EPS): Resin for Soft-Peel Protective Film
The resin is an all-acrylic polymer emulsion for use in removable, pressure-sensitive adhesive applications.
Engineered Polymer Solutions (EPS) has launched EPS® 2157, a resin for protective films for appliances, doors, and glass, as well as any application where protective masking is required. EPS 2157 is an all-acrylic polymer emulsion for use in removable, pressure-sensitive adhesive applications.
Ideal for film and tape market segments, this product reportedly exhibits moderate peel and tack with high shear values. The company reports that EPS 2157 distinguishes itself from other resins in this space, offering a “soft” peel as compared to other products with equivalent peel and tack that have a harder “zip-like” peel.