Applications include electronics, automotive manufacturing, shipbuilding, aerospace, military, and telecommunication.
Creative Materials recently introduced 111-27, an electrically insulating, thermally curing, colorless coating and encapsulant that can be applied by different methods. The product reportedly features excellent adhesion to polyimide, polyester, glass, and a variety of other high-energy substrates.
The company reports that, when used as a coating, 111-27 provides high strength and durability while maintaining performance during flexing and creasing. It also protects components from moisture, salts, and abrasion. 111-27 features high surface hardness, which reduces the risk of stress fracturing bonded components.