These adhesives reportedly make it possible to permanently adhere difficult-to-bond polymers to themselves and to other materials.
XlynX Materials recently announced the creation of a new class of adhesives the company is calling molecular glues. According to XlynX, these adhesives make it possible to permanently adhere difficult-to-bond polymers such as polyethylene and polypropylene to themselves and to other materials through strong chemical bonds.