Dispensing Equipment Reduces Production Time and Cost for Electronics Manufacturer
The two-part formulation is used to protect circuit boards and components from harsh conditions, such as moisture, high/low temperatures, and physical or electrical stress. Once potted in an enclosure, the unit is typically mounted on the chassis or drive train of heavy machinery such as a tractor or steer loader, where operating temperatures generally range from -40ºC to 85ºC (-40ºF to 185ºF). The potting operation is one example of a manufacturing process that has earned Phoenix products a reputation for exceptional reliability.
“Every time we set up a program, a ratio test is performed to check for variation,” he explained. “With this material, we could handle up to 5% deviation in the mix ratio, but during the nine months since we’ve acquired the FRC machine, the maximum fluctuation has never been anywhere near that,” Nyland added.