ND Industries has developed an improved seal for electrical conduit nuts. CONDU-SEAL is a molded, pre-formed seal made of PVC and is designed for use in harsh environments. ND CONDU-SEALs are available in bulk for customer assembly or can be factory-applied and heat-fused to the face of conduit locknuts. The ND CONDU-SEAL has been approved by U.L. and the C.S.A., and is available in diameters ranging from ½ to 2 inches.