This company has supplemented its range of Preventol P grades for in-can preservation with a number of combination products based on bronopol and isothiazolinone. In view of the fact that the use of chloromethylisothiazolinone is restricted by legislation to a maximum of 15 ppm, these products have the advantage of allowing this reliable active ingredient to be used further without the need for labeling.