ADM Tronics Unlimited Inc. offers a completely water-based laminating adhesive, Unex LT, specifically designed for use in the manufacture of PVC (vinyl) to nonwovens and paper wallcovering structures in a wet laminating process. This product can be used as supplied or diluted with water. It may be applied with conventional roller coating application, such as gravure, flexo, reverse-roll, rod, knife, etc. The product's rheology also allows for ease of application. Cleanup is achieved readily with water while the adhesive is wet; if dried, a higher pH cleaning solution is recommended.