Advanced Aromatics L.P., Houston, the leading producer of high-purity naphthalene and derivatives in the United States, has announced the expansion of its Baytown plant in order to increase the capacity of its naphthalene unit. The expansion, along with production technology improvements, will result in a 25% increase in naphthalene production capacity beginning in the third quarter of 2005.