ADM Tronics has announced the availability of a new water-based additive called Polaqua AD that greatly improves the performance of any aqueous ink, paint, adhesive, coating or resin. Flow, lay down, wet-out and many other characteristics are enhanced with only minor additions of this product to virtually any liquid. Polaqua AD works best when added directly to a customer's product and thoroughly stirred or mixed in. Addition ranges span from 1 to 10% depending upon the type of liquid and the degree of change desired.
For more information, call (201) 767-6040 or e-mail