Chemlok 6270 is a new adhesive that can provide improved bonding performance and mold fouling, as well as premium environmental and prebake resistance. Reportedly developed to improve process efficiency and quality in manufacturing applications, the adhesive can be used on seals, gaskets, bushings, mounts, industrial tires, rolls and rollers, as well as seismic and bridge bearing pads. With capabilities of bonding uncured rubber-to-metal substrates during the vulcanization of the elastomer, Chemlok 6270 can bond a variety of rubbers, including natural rubber, nitrile and EPDM to multiple substrates including aluminum, brass, and grit blasted or phosphatized steel when used in combination with Chemlok primers.