This company has completed its range of Gerbier HDS with a 35 g/m² low basis weight paper. The one-side coated glossy papers are used for flexible packaging. Compared to a standard Gerbier HDS 40 g/m², this new 35 g/m² grade reportedly provides a 12.5% weight reduction, enabling a lower environmental impact while maintaining high performance during lamination, printing, and converting.
Main applications reportedly include pouches or sachets for food and non-food end-uses such as sugar, coffee, aromatic herbs or dehydrated products. The papers offer the lowest basis weight on the one-side coated papers market for such applications.