The business will be included in H.B. Fuller's Americas Adhesives operating segment.
H.B. Fuller Co. announced today that, on January 27, it purchased the industrial adhesives business of Wisdom Worldwide Adhesives, a provider of adhesives for the packaging, paper converting, and assembly markets.
“We are pleased to welcome the employees and customers of this 140-year-old company to H.B. Fuller,” said Jim Owens, president and CEO, H.B. Fuller. “Wisdom’s highly successful go-to-market strategy, based on a focused product line, ultra-fast delivery and virtual service, will complement H.B. Fuller’s full value solutions. The acquisition will strengthen our leading position in this market segment within the Americas adhesive business.”