QUESTION: We tried to use a UV acrylic adhesive a few years ago to bond some clear plastic parts, but the cure was incredibly slow and excess adhesive on the outside of the joint remained tacky. Have there been any improvements in these adhesives recently?

ANSWER: In order to cure UV adhesives, you have to expose them to UV radiation. Many early UV adhesives had problems in bonding plastics, mainly because certain plastics don't transmit UV light very well, particularly those that contain UV absorbers to prevent UV degradation. Remember, if a plastic is transparent, all that really means is that it transmits the visible part of the electromagnetic spectrum and not necessarily the UV. You can check this out on your plastics by using a UV radiometer. In recent years, manufacturers have designed systems that can be cured entirely by visible light or sometimes a combination of UV and visible. Surface tackiness was a major problem in early UV adhesives because curing is inhibited by air in the atmosphere, which means that you don't get full curing at the surface. The tackiness can often be mitigated by using a mixture of different types of photoinitiators or by blanketing the parts with an oxygen-free atmosphere during curing. An alternative to this is to use an adhesive with a so-called "dual-cure" system that has a conventional UV/visible cure plus a cure system that reacts with atmospheric moisture to cure the outside surface. The most common way of doing this is to build some isocyanate functionality in the adhesive. Isocyanates will react with moisture just like they do in one-component polyurethane adhesives. There are some UV adhesives that are called cationic UVs, which involve the curing of a special type of monomers called cycloaliphatic epoxies and vinyl ethers. These adhesives are not inhibited by oxygen but are not as widely available as the more common acrylate systems.

Links

Did you enjoy this article? Click here to subscribe to Adhesives & Sealants Industry Magazine.

Dunn

Q&A Exchange is written by Dave Dunn, Ph.D., of F.L.D.Enterprises, a technical consultancy and full-service industrial market-research firm specializing in the adhesives, sealants, specialty rubbers and plastics fields. Dave is a former vice president and director of Loctite Corp. and has spent many years in troubleshooting adhesive and sealant problems. Questions for publication should be directed to him at 242 Trails End, Aurora OH 44202; phone 330-562-2930; fax (330) 247-1690; or email DrDave242@windstream.net .

Recent Articles by Dave Dunn

You must login or register in order to post a comment.

Multimedia

Videos

Podcasts

Environmentally Friendly Manufacturing

Edward Gotch, president of Emerald Kalama Chemical, talks about embracing sustainability with Susan Sutton, editor-in-chief.

More Podcasts

THE MAGAZINE

Adhesives & Sealants Industry Magazine

ASI May 2013 cover 100x133

2013 May

The 2013 May Adhesives and Sealants Industry Magazine includes articles about PPG and Bostik, as well as a Q&A about polyurethane. Check it out today!

Table Of Contents Subscribe

THE ADHESIVES STORE

handbook-sealant-tech.gif
Handbook of Sealant Technology

The Handbook of Sealant Technology provides an in-depth examination of sealants, reviewing their historical developments and fundamentals, adhesion theories and properties, and today’s wide range of applications.

More Products

asi1211p_Cover-DE.gifASI's Buyers' Guide

Annual purchasing resource for equipment used in the manufacture/formulation of adhesives, sealants, pressure sensitives, tapes and labels and for application of finished adhesives. 

Clear Seas Research

With access to over one million professionals and more than 60 industry-specific publications, Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40  youtube_40pxlinkedin_40