Franklin Adhesives & Polymers® has introduced a new pressure-sensitive adhesive, Covinax® 404, that is ideal for use with vinyl yet is versatile enough to be used on myriad other substrates.



Franklin Adhesives & Polymers®, a division of Franklin International, has introduced a new pressure-sensitive adhesive, Covinax® 404, that is ideal for use with vinyl yet is versatile enough to be used on myriad other substrates.

The division developed Covinax 404, a vinyl acrylic copolymer, specifically for use in adhering vinyl to other substrates. This newest Covinax adhesive is ideal for vinyl lettering applied on banners and other signage. It also works on metal and performs well in outdoor environments.

Covinax 404 also offers a rare balance of good peel and tack with high shear strength (approximately three pounds of peel and 3,000 minutes in shear), making it ideal for use as a permanent general-purpose adhesive. It works well on many substrates, including polyester, paper and vinyl.

The adhesive’s high shear strength also speeds up the die-cutting process by reducing adhesive build-up on cutting blades. Minimal build-up keeps blades dry and reduces printer misfeeds, increasing productivity in sheet-fed operations.

The new Covinax 404 is part of a line of removable, permanent and specialty pressure-sensitive adhesives offered by Franklin Adhesives & Polymers under the Covinax and Micronax® brands. These products offer varying degrees of peel, tack and shear for a range of end uses, from masking tape to automotive applications.

For more information, visit www.franklinadhesivesandpolymers.com.

Did you enjoy this article? Click here to subscribe to Adhesives & Sealants Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Podcasts

Environmentally Friendly Manufacturing

Edward Gotch, president of Emerald Kalama Chemical, talks about embracing sustainability with Susan Sutton, editor-in-chief.

More Podcasts

THE MAGAZINE

Adhesives & Sealants Industry Magazine

ASI June 2013 cover

2013 June

The 2013 June Adhesives and Sealants Industry Magazine includes articles about Nordson EFD and UV curing with lasers, as well as a case study on progressive cavity pumps. Check it out today!

Table Of Contents Subscribe

THE ADHESIVES STORE

handbook-sealant-tech.gif
Handbook of Sealant Technology

The Handbook of Sealant Technology provides an in-depth examination of sealants, reviewing their historical developments and fundamentals, adhesion theories and properties, and today’s wide range of applications.

More Products

asi1211p_Cover-DE.gifASI's Buyers' Guide

Annual purchasing resource for equipment used in the manufacture/formulation of adhesives, sealants, pressure sensitives, tapes and labels and for application of finished adhesives. 

Clear Seas Research

With access to over one million professionals and more than 60 industry-specific publications, Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40  youtube_40pxlinkedin_40