Resbond(tm) 931 graphite adhesive cures at 250 deg F to form 99%-pure graphite bonds that are electrically conductive and resistant to reducing atmospheres, most chemicals and solvents. The adhesive provides bond strengths in excess of 2,500 psi up to 5,400 deg F. It is ideal for repairing cracked or broken graphite trays, components, fixtures and dies. Circle No. 118