Loctite® 5203TM is a new, easy-to-service anaerobic gasketing material from Henkel Corp. that reliably seals close-fitting flanges against the same temperatures, pressures and chemicals as traditional liquid gaskets, yet removes easily without machining or chemicals. Used to bond and seal flanges in a range of equipment including engines, pumps and compressors, traditional anaerobic gasketing materials can be removed only with solvents or manual abrasion techniques.  

Ideal for use on frequently serviced flanges, Loctite 5203 eliminates the maintenance steps associated with resurfacing the flange as a result of scraping, sanding or abrasion. This anaerobic gasketing material resists low pressures immediately after flange assembly, even before the sealant is fully cured.

Loctite 5203 fully cures in 15 minutes to six hours. This red liquid ranges in viscosity from 50,000 to 100,000 cP and fills gaps to 0.010-inch without a primer, or 0.020-inch with the application of a primer.  This gasketing material withstands operating temperatures from -65° to 300° F.

For more information, visit www.henkelna.com/mronew.

Did you enjoy this article? Click here to subscribe to Adhesives & Sealants Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

ASI April 2014 Photo Gallery

Our April 2014 issue is now available!

Podcasts

ExxonMobil Tackifier Expansion

Dwight Tozer, vice president of ExxonMobil’s Adhesion Industry business, discusses the company’s latest tackifier expansion project with Editor-in-Chief Susan Sutton.

More Podcasts

Adhesives & Sealants Industry Magazine

ASI August 2014 cover

2014 August

Our August issue includes what is traditionally our most popular article of the year: the ASI Top 25. You won't want to miss it!

Table Of Contents Subscribe

THE ADHESIVES STORE

handbook-sealant-tech.gif
Handbook of Sealant Technology

The Handbook of Sealant Technology provides an in-depth examination of sealants, reviewing their historical developments and fundamentals, adhesion theories and properties, and today’s wide range of applications.

More Products

ASI 2014 Buyers GuideASI's Buyers' Guide

Annual purchasing resource for equipment used in the manufacture/formulation of adhesives, sealants, pressure sensitives, tapes and labels and for application of finished adhesives. 

Clear Seas Research

With access to over one million professionals and more than 60 industry-specific publications, Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40  youtube_40pxlinkedin_40 google+ icon ASI 30px