Hexion Completes Construction of Dispersion Manufacturing Unit

Hexion Specialty Chemicals Inc., a global supplier of water-based tackifier dispersions for pressure-sensitive adhesives, has completed construction of a new, state-of-the-art dispersion manufacturing unit at its production facility in Baxley, GA.

The new unit incorporates Hexion’s proprietary ROBUSTTM manufacturing process technology, which produces tackifier dispersions with finer particle size and virtually zero grit.

“This multi-million dollar capital investment further strengthens Hexion’s leading position in the pressure sensitive adhesives industry by enabling the manufacture of both higher solids and higher softening point tackifier dispersions,” said Brad Crocker, vice president, Global Ink and Adhesive Resins. “We now have the ability to operate at production facilities on four continents using the same ROBUST process technology, providing our global customer base with the highest level of product consistency and performance.”

For more information, visit www.hexion.com

Did you enjoy this article? Click here to subscribe to Adhesives & Sealants Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Podcasts

Environmentally Friendly Manufacturing

Edward Gotch, president of Emerald Kalama Chemical, talks about embracing sustainability with Susan Sutton, editor-in-chief.

More Podcasts

THE MAGAZINE

Adhesives & Sealants Industry Magazine

ASI May 2013 cover 100x133

2013 May

The 2013 May Adhesives and Sealants Industry Magazine includes articles about PPG and Bostik, as well as a Q&A about polyurethane. Check it out today!

Table Of Contents Subscribe

THE ADHESIVES STORE

handbook-sealant-tech.gif
Handbook of Sealant Technology

The Handbook of Sealant Technology provides an in-depth examination of sealants, reviewing their historical developments and fundamentals, adhesion theories and properties, and today’s wide range of applications.

More Products

asi1211p_Cover-DE.gifASI's Buyers' Guide

Annual purchasing resource for equipment used in the manufacture/formulation of adhesives, sealants, pressure sensitives, tapes and labels and for application of finished adhesives. 

Clear Seas Research

With access to over one million professionals and more than 60 industry-specific publications, Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40  youtube_40pxlinkedin_40