This company has developed BOSSR 319, a one-component, fast-cure, neutral oxime silicone sealant that is formulated to exhibit faster cure times and increased adhesion to a variety of materials. The product has a tack-free time of four to five minutes and quickly develops excellent green strength. It adheres to vinyl, wood, stainless steel, aluminum, glass and many plastics. Circle No. 153