New Products

PLASMATECH: Coating/Surface Treatment Process

PLASMAtech’s plasma enhanced chemical vapor deposition (PECVD) coating technology provides a “green” alternative for bonding or over-molding metal components.

Surface preparation of metal components prior to bonding incompatible materials may require caustic chemical etchants or other costly conversion coatings to ensure good bonding to the base metal substrate. By depositing a thin polymerized coating it is possible to create a tie or interface layer that permits direct bonding or over-molding to the metal surface. The resultant bond performance is excellent with results that often surpass those achieved with conventional methods.

Superior to other coating or conversion processes, plasma polymerized thin films can be deposited directly onto a plasma pre-cleaned substrate without exposure to the atmosphere. This continuous multi-step process provides excellent adhesion to the base substrate with the polymerization occurring at an atomic level.

PLASMAtech provides contract processing services, as well as a full line of low-pressure gas plasma and parylene coating equipment. Process development services are available for unique or especially challenging surface engineering requirements.

For more information, visit www.plasmatechnology.com.

Did you enjoy this article? Click here to subscribe to Adhesives & Sealants Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Podcasts

Environmentally Friendly Manufacturing

Edward Gotch, president of Emerald Kalama Chemical, talks about embracing sustainability with Susan Sutton, editor-in-chief.

More Podcasts

THE MAGAZINE

Adhesives & Sealants Industry Magazine

ASI May 2013 cover 100x133

2013 May

The 2013 May Adhesives and Sealants Industry Magazine includes articles about PPG and Bostik, as well as a Q&A about polyurethane. Check it out today!

Table Of Contents Subscribe

THE ADHESIVES STORE

handbook-sealant-tech.gif
Handbook of Sealant Technology

The Handbook of Sealant Technology provides an in-depth examination of sealants, reviewing their historical developments and fundamentals, adhesion theories and properties, and today’s wide range of applications.

More Products

asi1211p_Cover-DE.gifASI's Buyers' Guide

Annual purchasing resource for equipment used in the manufacture/formulation of adhesives, sealants, pressure sensitives, tapes and labels and for application of finished adhesives. 

Clear Seas Research

With access to over one million professionals and more than 60 industry-specific publications, Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40  youtube_40pxlinkedin_40