This company has introduced ERISYS EMUA-10, a thermoplastic, polyurethane-modified Bisphenol A epoxy resin. When cured, EMUA-10 provides tenacious bonds to PVC. Applications include vinyl flooring, vinyl sports surfaces, toughening modifier for other epoxy formulations, and modifier for improving thermal shock and peel resistance.