Victrex Polymer Solutions and Kuramoto Sangyo Co., a pressure-sensitive sheet manufacturer, have developed a high-resolution laser marking pressure-sensitive label using Victrex APTIV™ film. The VICTREX® PEEK™ polymer-based laser marking label is targeted for use in electronic and automotive label applications that need heat and chemical resistance, as well as for medical device labels that are used in high-temperature steam and chemical sterilization and cleansing processes.

The high-heat-resistant label uses heat-resistant acrylic adhesive with Victrex’s high-performance APTIV film as the substrate. The label can adhere to a range of surfaces, such as steel, ceramics and glass. The label is printed using the MX-V1000, a high-resolution laser marker made by the Omron Corp. A variety of label colors and thicknesses are available, including standard 50-micron and thin 25-micron label stock.

For additional details, visit www.aptivfilms.com.

Did you enjoy this article? Click here to subscribe to Adhesives & Sealants Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Podcasts

Environmentally Friendly Manufacturing

Edward Gotch, president of Emerald Kalama Chemical, talks about embracing sustainability with Susan Sutton, editor-in-chief.

More Podcasts

THE MAGAZINE

Adhesives & Sealants Industry Magazine

ASI May 2013 cover 100x133

2013 May

The 2013 May Adhesives and Sealants Industry Magazine includes articles about PPG and Bostik, as well as a Q&A about polyurethane. Check it out today!

Table Of Contents Subscribe

THE ADHESIVES STORE

handbook-sealant-tech.gif
Handbook of Sealant Technology

The Handbook of Sealant Technology provides an in-depth examination of sealants, reviewing their historical developments and fundamentals, adhesion theories and properties, and today’s wide range of applications.

More Products

asi1211p_Cover-DE.gifASI's Buyers' Guide

Annual purchasing resource for equipment used in the manufacture/formulation of adhesives, sealants, pressure sensitives, tapes and labels and for application of finished adhesives. 

Clear Seas Research

With access to over one million professionals and more than 60 industry-specific publications, Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.

STAY CONNECTED

facebook_40px twitter_40  youtube_40pxlinkedin_40