PPG Industries recently announced that it has entered into a technology license agreement with China-based Henan Billions Chemicals Joint Stock Co. Ltd., which reportedly provides Henan Billions the right to use PPG’s technology for the manufacture of chloride-grade titanium dioxide (TiO2) on a worldwide basis. The agreement completes the license of PPG technology previously announced by both companies.

“We are pleased to reach this worldwide technology license agreement with Henan Billions, as it should expand the global supply of chloride-grade titanium dioxide, as well as provide a commercial opportunity for PPG technology,” said Charles F. Kahle II, chief technology officer and vice president of Coatings Research and Development for PPG. 

Henan Billions currently supplies sulfate-grade TiO2 to PPG.

For additional information, visit www.ppg.com.

Did you enjoy this article? Click here to subscribe to Adhesives & Sealants Industry Magazine.

You must login or register in order to post a comment.

Multimedia

Videos

Image Galleries

ASI April 2014 Photo Gallery

Our April 2014 issue is now available!

Podcasts

ExxonMobil Tackifier Expansion

Dwight Tozer, vice president of ExxonMobil’s Adhesion Industry business, discusses the company’s latest tackifier expansion project with Editor-in-Chief Susan Sutton.

More Podcasts

Adhesives & Sealants Industry Magazine

ASI May 2015 cover

2015 May

You won't want to miss our May issue, with a special packaging-focused Adhesives at Work section, as well as coverage of pressure-sensitive adhesives (PSAs), biorenewable feedstocks, and more!

Table Of Contents Subscribe

Better Jobs

Is the economy prompting you to consider leaving your job for a better one?
View Results Poll Archive

THE ADHESIVES STORE

handbook-sealant-tech.gif
Handbook of Sealant Technology

The Handbook of Sealant Technology provides an in-depth examination of sealants, reviewing their historical developments and fundamentals, adhesion theories and properties, and today’s wide range of applications.

More Products

ASI 2014 Buyers GuideASI's Buyers' Guide

Annual purchasing resource for equipment used in the manufacture/formulation of adhesives, sealants, pressure sensitives, tapes and labels and for application of finished adhesives. 

STAY CONNECTED

facebook_40px twitter_40  youtube_40pxlinkedin_40 google+ icon ASI 30px

Clear Seas Research

With access to over one million professionals and more than 60 industry-specific publications, Clear Seas Research offers relevant insights from those who know your industry best. Let us customize a market research solution that exceeds your marketing goals.